Hi Experts,"Good Morning"My query has below.Help me to prepare pWPS.Process : GTAW +SMAWMaterial : P.No - 5BWhen we shall consider the impact test exemption.
ASTM A335 Grade P9.
Pipe Size - 16" Sch-60.
Thickness: 16.66 mm
Thickness range: 5mm to 33.32 mm
According to ASME B31.3 Table 323.3.1 shall I required an Impact for the above-mentioned thickness and material.
As per my knowledge, the above 25 mm impact test would be required.
How I can find according to line class where impact test required or not.
If a minus 29° C impact test not required for LAS.And regarding consumable for P No- 5A
ASTM A335 Grade P22 if I use ER90S-B3 ok or shall I use ER80S-B3 because my client suggest me to use ER80S-B3 please clarify way?Thanks in advanceRegardsKiran
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a5e2843d-2285-4e82-b631-6b73ea0b5aceo%40googlegroups.com.
Comments