Re: [MW:31177] Suitability of PWHT on ER309L Buttering over CS

309 weld metal may not be suitable for temperature above 370°C. Due to sigmaphase formation

On Wed, 22 Jul 2020 5:34 pm , <kunalenfield350@gmail.com> wrote:
Dear Experts

Need your expert advice that we have a joint of CS to SS, PWHT is applicable for CS. So planned to go for the buttering with ER309L & then PWHT prior welding with SS. Please advise does ER309L has any adverse effect on it if comes under the PWHT cycle applicable for P1 material.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/06110dfb-3346-4a70-bc6c-01f5fcf47d69o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO-BrE1mssrfd-bJXTqFxpfuMYzJQtkBHNeAVQTKf1uww%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...