Skip to main content

RE: [MW:31193] Re: Annealing and Normalizing temperature for F316 & SS410

Hello Suresh,

 

Please see the referenced standard and  important clauses as highlighted. You may read those and use your discretion to find solutions to your problem. If the problem is specific, then as suggested by Ramin Kondori, engaging a metallurgical specialist to find the correct solutions would be worthwhile and time saving for you organization.

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Aramco Approved Designated Project Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of SURESH
Sent: July 25, 2020 1:58 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31191] Re: Annealing and Normalizing temperature for F316 & SS410

 

Hi My question is what is the suggested annealing temperature for .ASTM A473 Typ410 grade. If your refer the standard of  ASTM A473, Table 2 they have given condition like A,1,2,3.

 

So if it is annealed condition what is the suggested temperature to achieve 223BHN?

 

 

Note: Refer attachment

 

Regards

Suresh

On Saturday, 25 July 2020 at 09:24:17 UTC+5:30 ramink...@gmail.com wrote:

If this is the TDC for raw material as per contract, then you have to find a supplier who can provide it unless you can prove that it would cause problems during fabrication or operation. And that is why I told you to provide us with more details. 

Then you need a qualified engineer who reviews all the documents and is able to get into a discussion with your client to find out whether other alternatives are acceptable or not. I do not think you can do it via online inquiries; you need to hire someone to do this for you... 

 

Ramin  Kondori

Sr. QA/QC & Welding Engineer

-----------------------------------------------------------

PG-Dip. in Welding Engineering (IWE  AT  0070)

BSc. in Civil Engineering (IUT)

BGAS Painting Inspector

ASNT Level I&II

                        

 

 

 

On Fri, Jul 24, 2020 at 7:45 AM <sathis...@gmail.com> wrote:

Dear Mr.Ramin Kadori.


My customer is given TDC for annealing at 955 C but raw material supplier is suggesting that they do only with 850 C. Its not for fabrication, to give raw material into finished component by machining. Required hardness is 160 BHN

As per ASTM A473, Grade/Typ. 410 can be supplied as per the following conditions:




Condition A refers to annealing. (ASTM A473 mentioned with A, 1,2,3,). In this case how to determine the Annealing temperature?


My requirement is to get hardness of 160BHN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bbae9d88-9b64-421b-9dc6-8b8c357732d9n%40googlegroups.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...