Hi,

There are two scenarios:

1.       The tank is new construction: it doesn't seem to be a good practice; it creates complications to make bending on the pad plate, extra stress on the pad plates and also it may result in poor welding advise the designer to combine the two pad plates and make it one.

2.       The tank is in service: if you don't have any repair on the area of the said plates, just ignore it. If you have repairs on the pad plate area you can switch to scenario one and combine the two pad plates into one pad plate.

 

With best regards,

Firoz Ahmed (Umar), PMP®, MICorr®, Sr Corrosion Technologist

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jayadeep C
Sent: Sunday, July 19, 2020 12:18 PM
To: materials-welding@googlegroups.com
Subject: [MW:31156] Distance between the welding of pad plates in storage tank as per API 650

 

Hi,

 

 Any one please clarify What is the solution if a pad plate crosses over another pad plate in the storage tank shell/roof? Anything mentioned in API 650?

 

Jayadeep

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGR-dAtVRF9LsC1xbdW424oQseSULbg6VPZ6gRxDyVGj5Xa3EA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...