Thursday, July 23, 2020

[MW:31179] RE: 31176] Suitability of PWHT on ER309L Buttering over CS

Hi Kunalenfield,

 

You may use 309L for buttering on carbon steel and subsequent PWHT, provided the design conditions do not exceed the recommendations of API RP-582 as below. A buttering PQR should be established according to ASME Sec-IX , QW -283 . Typical buttering thickness to lesson the effects of welding on the buttered surface should be 3/16". Read the details of QW-283 to establish a buttering followed by welding on the same test coupon.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of kunalenfield350@gmail.com
Sent: July 22, 2020 7:54 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:31176] Suitability of PWHT on ER309L Buttering over CS

 

Dear Experts

 

Need your expert advice that we have a joint of CS to SS, PWHT is applicable for CS. So planned to go for the buttering with ER309L & then PWHT prior welding with SS. Please advise does ER309L has any adverse effect on it if comes under the PWHT cycle applicable for P1 material.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/06110dfb-3346-4a70-bc6c-01f5fcf47d69o%40googlegroups.com.


Virus-free. www.avg.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...