Sunday, November 10, 2019

Re: [MW:30219] Hardness Test

Dear Venkat,

Please refer API RP 582 for the same.

Thanks & Best Regards,
Rajnish
On Wednesday, 6 November, 2019, 10:17:12 AM GMT+7, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:


Dear All,
Pl clarify, how to take hardness measurements on welds after PWHT for SA 516 Gr 70 material.
Is there any code reference?

Thanks& Regards,
Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHYCPSu_LL3RaVz%2B7Q10FSw8dED8kXGn_y9oWQyFoTs4A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/829371129.1292042.1573351719172%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...