Re: [MW:30205] Mechanical test for Welder qualification

So we have to all the destructive test as mentioned in Api 1104 section 5.4??????

Pls confirm 

On Thu, Jan 31, 2019, 5:34 AM Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gents,

Is it mandatory mechanical test qualification for welders as per ASME B31.8 sour gas service requirement as per clause B823.2?.

Qualification by RT is acceptable ?.


Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKCULh7KJw%2BVtTO0DU6aDYTZHRTOQ_WetA%3DexrCg-4_Dh8UBsg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...