[MW:30228] Impact test Requirements

Dear All,

Can any one describe me regarding Impact test requirement as per code ASME B31.3 ASME Sec VIII, API 582 and NACE 472 .

What is the thickness limits? and how i can I know that the piping line class required Impact test or not?

As per piping class what are the thing to I have to check?

And please describe me regarding ASME B31.3 Table- 323.3.1?

For stainless steel above 25 mm where required Impact test or Not?

Thanks In advance.

Regards 
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/86e3be16-154b-4460-937e-034782095f04%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...