In case of impact test requirements it is a supplementary essential variable. So the max. limit in this case is 195degC. Check QW-406.3 and the tables in article II
Στις Δευ, 1 Απρ 2019, 10:17 ο χρήστης pradip kumar Sil <pradipsil@gmail.com> έγραψε:
Inter pass Temp. is not the essential variable and as I know there is no such criteria for Max. and minimum inter pass temp. limit. If your test coupon pass required DT ( Tensile Test, Face Bend, Root Bend) , there is no problem--On Sun, Mar 31, 2019 at 7:56 PM George Dilintas <dilintas@gmail.com> wrote:your max Interpass temp in the WPS is 195degC.Pls take into account that the Code is not a welding handbookΣτις Παρ, 29 Μαρ 2019 στις 5:35 π.μ., ο/η Souravbohray <ermechsouravbohray@gmail.com> έγραψε:i want to know were is given asme sec 9 what will be interpass temprature.is there any value given in code for interpass temp it is given only + 55 c but what temperature we can go +55 c preheating temp given in asme sec 8--
On Tuesday, 14 September 2010 18:13:18 UTC+5:30, limesh M wrote:Dear All,
Design Code: ASME B31.3 Welding Code: ASME SEC IX
I have a Low temperature carbon steel impact tested PQR with a PWHT range of 600⁰±10⁰C.Is this condition giving an exemption for me on QW406.3 to prepare a WPS with maximum interpass temperature of 200⁰C.
Maximum interpass temperature observed during specimen welding: 140⁰C
Regards,Limesh
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
----Dr. Georgios Dilintas,Dipl. Ing. In Aeronautic and Space EngineeringPh.D in Mechanics of Solids - Computational MechanicsA.I.S, A.N.I, IRCA Lead AuditorWelding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments