Pl share your opinion on PWHT requirements for Cladded ( CS+SS clad ) boot shell / head which is connected by flange. 



1. PWHT is required for clad portions ? even the service requirement calls for PWHT ? or 
2. PWHT can be waived off as per NACE MR0175/ISO 15156-2 Clause A 2.1.2 , A 2.1.4, , Table A1, Clause A 2.1.5 (b) & NACE MR0175/ISO 15156-3 Clause A 13.1 ?

Looking for Aramco reference, 

Pl share your opinions


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...