Re: [MW:29505] Geometric Unsharpness and discountinuity size rel

Answer is  NO 
To minimise the unsharpness code given acceptable value. 


On Mon, 22 Apr 2019 at 3:28, Hareesh K V
<hareesh13h@gmail.com> wrote:
Dear Group Members,

Related to : Radiography Examination 

Can we add the value of geometric unsharpness to the discountinuity size acceptability value for accepting a discontinuity. 

Governing codes: 
ASME BPVC Sec V & ASME B 31.3

Example. 

Say Up to 2mm porosity is acceptable as per the code.

We have established the geometric unsharpness value by procedure qualification of the technique and observed as 0.2

My question is, can we accept a porosity of 2.4mm by adding (0.2x 2times Ug for both the sides of the discountiuity) the geometric unsharpness to the acceptability value of 2mm.

Please advise with code references or code interpretations. 

Regards, 

Hareesh K V
8547859202

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...