Monday, April 29, 2019

[MW:29531] Impulse Tube and Pipe -SS 316

Hi,
What is the differenc between a SS Impulse tube and SS pipe .
We have used 1/2" inch Pipe instead of Impulse tube ,with the thickness satisfying the Pressure requirements.Does it will affect the operation of the lines since we had to bend these pipes as per the requirement.
As far as I know ,the material properties are same for both pipe & tube ,only thickness varies in tubes depends on the design requirements and for pipe we have to take the matching sizes with respective SCH from the standards.

Also is there any difference in manufacturing or in properties of Impulse tube from normal tubes , or it is the same tube but only called as impulse tube based on application.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...