Re: [MW:29542] A 234WPB

 Can use upto temp 425 0c. 

Regards 
Anand gupta 
ThyssenKrupp 


On Tue, 30 Apr 2019 at 17:05, krishna kamal nayan Pandey
<kkmech1987@gmail.com> wrote:
Gents,
Can anyone confirm the temperature range of A 234 WPB fittings. 
I mean the temperature this grade fitting can resist?

Best Regards,

 

Krishna Kamal Nayan  


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...