When you are using SS sheets, you cannot expect to have zero gap between base and cladding...
With overlay welding, that is possible but with this method, no.

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Sun, Apr 28, 2019 at 6:48 AM 'Ali Bhatti' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear experts

We are preparing a tank for use of Caustic Soda (NaOh) with inside SS cladding for cladding we will use SS sheet after fabrication. Above I forwarded query of our client. Can u give ur suggestion against query. Main point is that how we can sure zero gap between MS & SS

By UT strainght beam method. To check lack of bonding between cs and ss
Sent from my iPhone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...