Tuesday, April 23, 2019

Re: [MW:29508] How to make WPS and PQR for A106 Gr. B for my study


El lun., 22 de abril de 2019 9:35 p. m., Kamal Basha <basha2070@gmail.com> escribió:
S 8inch thickness 

On Sat, 20 Apr 2019, 7:57 a.m. Vinay Thattey, <vinay.thattey@gmail.com> wrote:
PLEASE SPECIFY .Is job thickness 8 "??

On Thu, 18 Apr 2019 at 08:05, Kamal Basha <basha2070@gmail.com> wrote:
Sir 

please tell me what is the thickness range for 8 inch and above.








On 16 Apr 2019 7:48 a.m., "Vinay Thattey" <vinay.thattey@gmail.com> wrote:
The thickness range is 1.5 mm to twice the thickness ( 2 x 5.9) . 
Please read  ASME B & PV code Sec IX  QW 450 ( Specimen and table) and notes 1 to 5 of this table.  Also read QW_403 .

On Fri, 29 Mar 2019 at 09:05, Emil Multazam <emil.multazam@gmail.com> wrote:
Dear Experts..

Could anybody help me, how to determine range thickness pipe A106 Gr.B for WPS ?
I have test coupon with thickness 5.9mm

Regards,

Emil Multazam
Manufacturing Engineering
College at University of Surabaya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...