check

ASME B 31.3 328.5 Welding Requirements for tack weld qualifications.
328.5.1 General
(c) Tack welds at the root of the joint shall be made with filler metal equivalent to that used in the root pass. Tack welds shall be made by a qualified welder or welding operator. Tack welds shall be fused with the root pass weld, except that those that have cracked shall be removed. Bridge tacks (above the weld) shall be removed.

and check QW-452.6 for Fillet Qualification by Groove‐Weld Tests.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

(55:33) O company of jinn and men, if you have the power to go beyond the bounds of the heavens and the earth, go beyond them! Yet you will be unable to go beyond them for that requires infinite power.

 
Date: 2018-11-28 18:49
Subject: Re: [MW:28702] Tack weld
Yes as per QW-452.6

On Wed, Nov 28, 2018, 5:46 PM gurupad sugavi <gurupadgs@gmail.com> wrote:
Dear gents

Please clarify about the following 

If a welder qualified in 3g plate, can he weld pipe tack weld at any position?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...