Re: [MW:28656] ER80S-D2 and ER80S-G selection- GMAW

Hi,

Greetings,

Why you are going for G?

What is your BM?

You are right G has lot of disadvantages where W.E has to quote the requirements between your company and supplier and again you have to get approval from your client, so its bit risky.

G maybe used for special purposes.

You are right with D2 and it is acceptable highly recommended as per your BM. 

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 & AWS-CWI (2007)
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

Say (O Muhammad SAW to mankind). "If the sea were ink for (writing) the Words of my Lord, surely, the sea would be exhausted before the Words of my Lord would be finished, even if we brought (another sea) like it for its aid."18-109

 
From: Ri@z
Date: 2018-11-21 11:50
Subject: [MW:28655] ER80S-D2 and ER80S-G selection- GMAW
Hai Experts,


Among ER80s-D2 and ER80s-G , which one is better choice for GMAW auto welding  ? 


I read that D2 is particular to eliminate porosities arising due to CO2 shielding gas


I didnt find aby advantages of 'G'  filler wire.


Pls help


Riaz

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...