Yes its not clear.
If i am not wrong check Interpretation: IX-10-34, for your scenario.
Thanks.
Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 & AWS-CWI
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
Say (O Muhammad SAW to mankind). "If the sea were ink for (writing) the Words of my Lord, surely, the sea would be exhausted before the Words of my Lord would be finished, even if we brought (another sea) like it for its aid."18-109
Jibin ,Your Question is incomplete , please brief clearly your requirement .SureshOn Wed, Nov 14, 2018 at 3:44 PM Jibin Philip <jibinphilip123@gmail.com> wrote:Dear Experts..
code asme sec 9 ,B31.3 .. pqr test plate thickness is 20 mm ..need charpy test .. so what will be thickness range qualified ??
Regards,
Jibin
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
----Thanks & Best Regards,
Suresh Paidi
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments