I prefer you to go with more stringent, if you have owners special requirements , and check below para 812 MATERIALS FOR USE IN LOW-TEMPERATURE APPLICATIONS, Whenever the minimum design  temperature is below −20°F (−29°C), a fracture control program shall be established. The program shall address parent materials, the parent material seam weld  (if present),circumferential butt welds, attachment welds, and any weld heataffected zone (HAZ) and 841.1.2

Thanks,

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

(6:59) He has the keys to the realm that lies beyond the reach of human perception; none knows them but He. And He knows what is on the land and in the sea; there is not a leaf which falls that He does not know about and there is not a grain in the darkness of the earth or anything green or dry which has not been recorded in a Clear Book.

 
From: Ri@z
Date: 2018-11-24 11:17
Subject: Re: [MW:28678] Impact requirement of multiple process and different Group number
This is for station piping pertaining pipeline , construction code is B31.8.

Our client  Spec required  -45 degree impact at LTCS material , where all material belongs to P1G1.  And remaining material/Class required impact @-20 degree. For minimize PQR  I have proposed P1G1#P1G3 combination. Impact of  Weld and G1 HAZ will carry out in -45 degree and G3 HAZ will be carried out in -20 Degree . 


Is it Okay in Code and technical point of view , right ? 

Riaz 

On Friday, 23 November 2018 09:13:49 UTC+5:30, George Dilintas wrote:
What is the construction Code?
Pls note that Section IX does not deal with impact test at all

Στις Δευ, 19 Νοε 2018, 09:40 ο χρήστης Ri@z <riaz.r...@gmail.com> έγραψε:
Dear All, 


PQR conducted on P1G1#p1G3 with wall thickness 7.8 mm. Root Hot Pass with GTAW and Remaining SMAW. 


1) Is this required to carry out impact test of HAZ for both G1 and G3 material ?

2) Is it required to carry out impact test for both GTAW and SMAW process separately ??


With Regards

Riaz  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...