Re: [MW:28660] Electrode brand change

If the initial PQR was done with filler metal classification without the letter G at the end you don't need a new PQR

Στις Παρ, 16 Νοε 2018, 07:45 ο χρήστης HARISH VARUDE <harish.varude02@gmail.com> έγραψε:
Dear All Expert.

With reference to the above subject,our contractor want to change electrode brand and manufacturer.

So I would like to know should I need to create new Welding procedure again due to changes in electrode brand and manufacturer?

Please let me know about this query.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...