Re: [MW:28625] Thickness range for PQR

Jibin , 

Your Question is incomplete , please brief clearly your requirement . 

Suresh 

On Wed, Nov 14, 2018 at 3:44 PM Jibin Philip <jibinphilip123@gmail.com> wrote:
Dear Experts..

code asme sec 9 ,B31.3 .. pqr test plate thickness is 20 mm ..need charpy test .. so what will be thickness range qualified ??
Regards,
Jibin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Thanks  & Best Regards,

Suresh Paidi


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...