Dears,

Our prospective vendor is offering TOFD for category A & B weld joints instead of RT for a process column due to RT room size limitations. Is it acceptable by ASME SEC VII DIV-1? What will be the joint efficiency in this case to be used in calculations?

On Tuesday, 4 December 2012 22:11:36 UTC+5:30, Nitin Shetty wrote:
Dear Mohammed,

Both have advantages and disadvantages over each other. PA funda is similar to conventional UT and the no of crystals are more or in other words the angles used for scanning is more in PA compared to conventional UT. TOFD cannot be used on category D joints. Sensitivity wise TOFD is better than PA.

Regards,

Nitin

On Fri, Nov 30, 2012 at 11:46 AM, mohd <mohd...@gmail.com> wrote:
Dear all,

What is different between TOFD& PAUT?
which one is better?

regrds,
mohammed.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...