No never n cant. Really u know mean of wps. wps is a written guidline to welder to how to do welding with ranger of variables. Suppose u take material A so u select all the parameters according to chemical , mechanical prop of material A.
But now u want to do welding of material B ie mechanical prop chemical prop are diff u have to guide ur welder on diff ranges diff parameter of variable so parameter n ranges are diff for both material A and B ie u have to make separate wps for both material.
Generally if prop are similar but name of material is diff than also u have to make diff wps.
But u are using diff process ie smaw welding for root saw for 1st layer gtaw for 2nd layer and so on for that u have to memtion that all on same wps for each material A and B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...