General information only.

 

Attached AWS standard may be useful for your reference. ( AWS UGFM – User's Guide to Filler Metals)

Refer PART E: COPPER AND COPPER-ALLOY for your reference.. 


Also refer SFA-5.6/SFA-5.6M & SFA-5.7/SFA-5.7M 

 

Also look for your regular consumable supplier recommendation or recommended filler metals selection guide from various consumable manufacturers like M/s. ESAB, ADOR, BOHLER, LINCOLN, KOBELCO & AIR LIQUIDE etc. etc.…

  

Ensure Weldability / metallurgical  compatible. 

 

As u know, You need to have qualified procedure between P.No 1 to P.No (31 -35 – copper and its alloys) on your requirement basis.

 

In case buttering / overlay on CS side, qualify the procedure in same way…








On Sun, Mar 18, 2018 at 6:34 PM, Karunakaran Karan <karunaqc@gmail.com> wrote:
Dear Experts,

            Have one doubt regarding copper to carbon steel,which filler using this kind of welding .And explain code also


*S.KARUNAKARAN*
  karunaqc@gmail.com




Dear

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...