Re: [MW:27578] Re: If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?
A-No is not essential for performance qualification.
2018-03-24 12:55 GMT+02:00 Vairamuthu <vaira.muthu.78@gmail.com>:
As Mr. Chandra is clearly said the welder can't weld in CS as code very clear on this and very nicely explained by Chandra Ji. which is copied below.Dear Team,Both the carbon and stainless steel filler metalsFno. is 6.Refer QW-404.15 (A change from one F-no in tableQw-432 to any F-number or to any other fillermetal, except as permitted in Qw-433.Qw-433 table says qualified with any F.no6 qualifiedFor all F-No 6 [refer note1]Note1 says: deposited wels metal made using abare rod not covered by an SFA specificationbut which conforms to an analysis listed inTable QW-442 shall be considered to be classifiedAs F-no 6.Means carbon steel F.No 6 (but A.No is 1)Stainless steel F.No 6 (but A.No is 8)So, even F.no same but weld metal analysis isdifferent. So he was not qualified to weld stainlessBest Regards,Chandra
On Saturday, February 24, 2018 at 1:03:47 PM UTC+3, PK wrote:Dear Sir,If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW? Need code Referance...Thanks.PKM--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments