Re: [MW:27573] Tapering for diffrerent Mat. thickness

Pls 2 is correct. I don't know why somebody is referring you to B31.3.

Regards

Rems

On Tue, 27 Mar 2018, 06:57 Kamal Basha, <basha2070@gmail.com> wrote:
U have reference in b31.3

On 25 Mar 2018 11:51 a.m., "Nallavan" <gane2478@gmail.com> wrote:
Dear Experts

Design/Const. Code AWS D1.1.

Approved Engineering Drawing calls for 1:4 Ratio for transition thickness base material


My understanding - 2 is correct.

Pls refer attach and advise if  1  or  2 is correct.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...