Wednesday, March 28, 2018

[MW:27578] Impact test of plates for pressure vessel

What is imp criteria for impact test of any kind of raw material using pressure vessel fabrication. How to know we have to do impact test of raw matetial using for pressure vessel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS