If you are working with ASME IX and both materials are P8, you can use the same WPS without problems, but verify that two data first.
2018-03-30 8:05 GMT-06:00 chiluka venkatramulu <ramuluchiluka@gmail.com>:
--VenkatWith best wishes,Shall I need to prepare other WPS based on the above PQRORDear All,Pl clarify the below.
Can I Use SA240 TP 304 WPS to weld SA240 TP 316 material
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
Ing. José Juan Jiménez Alejandro
Soluciones en Soldadura e Inspección
Cel. 812 352 4606
Skype: jjjimeneza
Twitter: @jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments