Re: [MW:27506] WELDING ff gfU hGuUUCONTINUITY FOR WELDER

Dear

Thanks for the explanation and guidance.

Kind regards

On Mon 12 Mar, 2018, 15:14 Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Welder/Welding operators continuity ONLY for their Qualified Welding Process. Whether you do overlay, build up or fusion weld

On Mon 12 Mar, 2018 1:10 pm Nachhattar Singh, <nachhattar1947@gmail.com> wrote:
Dear
Thanks for the information, but my main concern is about the reference that this is the requirement for ONLY FOR OVERLAY / HARD FACING OF WCB material.

Kind regards
N S Gurm

On Mon 12 Mar, 2018, 12:55 Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
1. Prepare welder/welding operator Log, in this, once in a 15days or weekly enter the Process, Job description etc.
2.Prepare  welder/welding operator continuity record on monthly basis with respect to welder log.

Virus-free. www.avast.com

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, Mar 12, 2018 at 11:20 AM, Nachhattar Singh <nachhattar1947@gmail.com> wrote:

 

Dear Experts

 

Want to have an information as one of the auditor has given a Major NCR on-

 

"welder continuity for the welder not maintained"

Whereas the welding requirements for the organization are only the 'overlaying with 13% CR (crome) only

and that too the same welding does perform this activity on regular basis'.

 

Please give the reference code/standard reference if the welder continuity is

required to be maintained under these circumstances.  

 

Thanks in advance.

 

NS Gurm

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...