I agree with Rems Okonkwo. Please find below the snap shot of ASME Sec.IX

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Wednesday, November 29, 2017, 2:15:21 PM GMT+4, Rems Okonkwo <rems.okonkwo@gmail.com> wrote:


If there is no requirement for impact test according to your design parameter and all other things being equal, the WPS qualified for ASTM A106 to AISI 4130 can be use for welding of ASTM A 105 to AISI 4130.

Regards,

Rems Okonkwo
Welding and Materials Engr
IWE Nigeria

On 28 Nov 2017 13:07, "varun625" <varun.ndt@gmail.com> wrote:
Dear Experts,
I have a WPS qualified as per ASME Sec IX for ASTM A106 with AISI 4130.Now we have a requirement to weld A105 with AISI 4130. As I understand 4130 is unlisted material as per ASME and we need to qualify WPS every time. Kindly confirm the same or advice. Or can I go ahead with same WPS as there is no requirement for Impact testing. 
Thanks in adv.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...