Dear Experts,

Attaching Joint details. 

Thanks & Regards

Subrata Das
Mob: +91-9828160168

---------- Forwarded message ----------
From: Subrata Das <subrata19732111@gmail.com>
Date: 18 November 2017 at 15:27
Subject: Fwd: [MW:27006] WPS REG
To: subrata.das@blissanand.com



Thanks & Regards

Subrata Das
Mob: +91-9828160168

---------- Forwarded message ----------
From: Karthik <karthik6684@yahoo.com>
Date: 18 November 2017 at 14:54
Subject: Re: [MW:27006] WPS REG
To: Materials & Welding <materials-welding@googlegroups.com>, Subrata Das <subrata19732111@gmail.com>


Hi,
Please find below the Code interpretation. 

Question: When nozzle or branch connections are attached to the wall or head of a pressure vessel, what are the basic criteria establishing procedure and performance qualification?

Reply: For groove weld procedure qualification, the base metal thickness range for all base metals being joined in addition to the deposited weld metal thickness range for each process used must be qualified in accordance with QW-451 (see QW-202.4). Also, see exemptions in QW-202 for fillet weld procedure qualifications. 

Thanks& Regards,

 

(Karthik)


Mobile: +66 892512282 
E-mail : k
arthik6684@yahoo.com



On Saturday, November 18, 2017, 4:07:17 PM GMT+7, Subrata Das <subrata19732111@gmail.com> wrote:


Dear Experts,
Please guide me for test coupon thickness to be considered for below case

- Vessel thickness 14.27mm
- Nozzle thickness 40mm
- Set in type Nozzle on Vessel shell
- Full penetration weld with fillet
- Impact test applicable
- No PWHT

Do I need to consider Nozzle thickness 40mm or Shell thickness 14.27mm. Appreciate your reply in advance with Code clauses.

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...