Please refer the attached Macro Photograph extracted from the single PQR test Coupon & Joint Preparation details. The thickness of test Coupon is 30 mm Grade of Material S460 ML & backing plate with 10 MM same Grade. The Weld Process is FCAW. PQR qualification is according to AWS D1.1 2015.

Based on the attached please clarify the Below comments is the Result to be Passed or Reject.

1)     As per the Weld Joint Preparation is "Single Bevel" But after welding it seen like "Single Vee" with other side bevel of 10° What Joint configuration will be Considered in the PQR / WPS as Result  

2)     The attached Macro Photograph is seen that Root is not Penetrated with Backing Plate. – is this Result shall be Passed or failed. 

Waiting for your valuable Response / comments with explanation stating Passed or Failed.  

Regards,
HIREMATH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...