[MW:27002] AISI 8620 Welding_WPS PQR reg

Dear all,

I have to qualify a procedure for AISI 8620 material.

Material:AISI 8620
Welding Process:SMAW
Purpose of Qualification: For valve repair
Code:ASME SEC IX

I want to know the following

1) Electrode
2) Preheat
3)PWHT requirement
4) AISI 8620 - Unlisted material or If it comes under listed material want to know the P number & group number.

Siva



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...