​Dear Pradip,
Thank you for the excel table and your time.
Please note that API-1104 Some of defect/flaw contractors will accepted reference of your table.
The API-1104 code allowed the range of below defects/flaws,
Lack of fusion - up to 25mm in (300 mm) length of weld.
Lack of penetration - up to 25mm (300 mm) length of weld.
Undercut - up to 50mm (300 mm) length of weld.

Kindly refer the code and please take your account in next version.

Thanks,
Best Regards,

Dominic V.K.




On 19 November 2017 at 11:17, Engineer Inam-Ul-Haq <engrhaq673@hotmail.com> wrote:

Very Nice, Mr. Pradeep Ghosh




From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Pradip Ghosh <pradipg2@gmail.com>
Sent: Sunday, November 19, 2017 11:59 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27011] Re: Radiography acceptance criteria.
 
 Dear ,Shashank C Vagal  use bellow link to download the file.

https://drive.google.com/open?id=0ByvRBXye0uymdW9aekp1M0J1cHc

On Fri, Nov 17, 2017 at 11:49 AM, 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Pradeep Ghosh,
Please fwd to me a copy of this excel program .
 
Thankfully Yours,
Shashank C Vagal  
301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
 


On Friday, 17 November 2017 9:15 AM, SULTAN <sultanhyder0@gmail.com> wrote:


Very Nice effort  Mr.Goshi
i think one thing is missing in this is ASME Sec.I

Thanks,

Regard's
Sultan 
QC Engineer 
MEC Engineering

On Thursday, September 5, 2013 at 3:18:52 PM UTC+5, Pradip Ghosh wrote:
Dear All,

I have prepared a excel program in which you can find Radiography acceptance criteria of ASME Sec IX,API-650,API-1104,ANSI B 31.3 and ASME Sec VII Div  in a click.
Please give me your review and comments.




Pradip Ghosh

QA/QC Engineer
Mott MacDonald (P) Ltd.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/k5wvDu0g8dU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards,

Pradip Ghosh
QA/QC Engineer
Mott MacDonald (P) Ltd

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...