[MW:27081] RE: 27063] CTOD and SSC requirements for welding consumables

Hi Yokesh,

 

It's a very specific requirement for pipeline welding. Which client or what specification no you're referring to?

Appreciate your response.

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of TDK YOKESH
Sent: November 28, 2017 1:38 AM
To: materials-welding@googlegroups.com
Subject: [MW:27063] CTOD and SSC requirements for welding consumables

 

Dear experts , 

 

We are performing auto GMAW using ER70S6 ( hobbart ) on pipeline job ( X65 with SMYS >450Mpa . As per B31.8 /31.4 PWHT is to be done for thickness above 32mm. Our pipeline thickness is 33.3, 44.45 and 50.2mm . Now client requires CTOD and SSC values of welding consumable  after PWHT . Which code or standard demands for it ? Where can I refer for the CTOD and SSC requirements ?

 

Thanks and regards

TDK Yokesh 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...