[MW:27064] B31.1 pwht for P11 WELDOLET requirement.

hello.
I need to know about PWHT time for RUN PIPE 16" S120 to 8" S120 P11 WELDOLET PWHT hold time. if anyone know how to figure this time please guide me.
thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS