Tuesday, November 21, 2017

[MW:27028] PWHT thickness requirements

Section VIII div.1 and div.2, B31.1, B31.3, etc all have a minimum thickness range(s) for PWHT. In particular for carbon steel.

The question I had was, what is the theory behind the chosen thickness? Same being for non-mandatory PWHT rules like "groove welds not over 1/2", etc

Where do these thickness originate?

Another question, why do the electroslag welds in ferritic materials in materials over 1 1/2" have to be "grain refined by heat treatment"? besides preservation of the material and things like that.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...