Wednesday, April 12, 2017

[MW:26391] Re: Requirement of Solution Annealing for SS DIshed head after forming

Hi All,

I have read all the valuable discussion happened here, I come to know about few point what I was not aware thanks all of you.

I have a torispherical dish head with fiber elongation of 6%, Design temperature =200°C, MOC = SA-240 Gr. 316L . As per UHA -44 weather Solution annealing is required.

The point behind asking this question is if the design temperature is below 580°C (as given in Table UHA-44) then do I need to solution annealing.

Second thing As per clause UHA-44 (a) 1 (-a) what is finishing -forming temperature. I believe it is not design temperature.


 
On Tuesday, 13 September 2011 15:48:03 UTC+5:30, asad azmi wrote:
Dear All,
 
Greetings.
 
SS Vessel is being fabricated as per construction code - ASME SEC VIII DIV 1
 
SERVICE : SOUR Service
 
Material of Construction  for Dished Head - SA 240 316L, 20 mm Thickness.
 
I  believe stresses will be  induced in the material  during forming and as a result , Sulfide Stress Cracking (SSC) failure may occur during operation.
 
Whether Solution Annealing of SS Dished Head is required after forming?
 
Please give reference of any International Standard.
 
Thanks & Regards
 
Asad Azmi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/85cb5b61-041b-4564-a6d4-ce7b9c608dfe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...