Hello, 

 For the calulcation of electrode consumption for welding of any type of steel structure, you need to know welding metal deposition on those structures.  so you need to calculate first the weld metal deposition on it. after that based on the suitable multiplying factor with this  weld deposition you will get the welding electrode consumption.

welding electrode consumption = multiplying factor x weld deposition

for calculation of weld deposition, One andriod/window application is developed by me it would be helpful to you 
" Smart welding Solution ( free)"- google play store . there is also paid version. but  for initial stage you can use this free version.
with this you can   get various information which will helpful for welding calculation. 

weld deposition/ volume/cross section area/ surface opening of any type of groove joint configuration including fillet.
it is also developed for overlay application. 
there is toturial section also for understanding. it is highly comprehensive  so it might take time to understand. 
you can also save these information in pdf also.


 Hope it would help you

Regards
Rishikesh kumar


On Fri, Apr 21, 2017 at 10:38 AM, Neem Lal <neem4u@gmail.com> wrote:
Hello experts,
I want to know, how we can calculate electrode consumption for welding of conveyor gallery steel structure, elevated at 10 meter height and span length of 100 meter about.
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/63fa2fc2-3f9f-4c02-9c09-fe70d8b84523%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXs1KoAjEjchMiX%2BS698aCgZZX-wK1F4hDiL1mDpuKiqHgOdA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...