Sunday, April 16, 2017

Re: [MW:26425] RT-Penalty Joints

Refer ASME B31.3 Chapter VI -341.3.4 Progressive Sampling for Examination.

Reagrds,

G.S.Perumal.


On Mon, Apr 10, 2017 at 12:09 PM, JIJILAL K M <jijilalkm2@gmail.com> wrote:
Dear Experts,

Please enlighten, is it specifically mentioned in code for 2 penalty joints for 1 repair (same welder)?

construction codes are Asme B31.1&31.3.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHi3MGwOKC0zeDMMt%3D3aPUrzQqntf5skw9aedqZhyX0Scw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPFTRW%3DC7YghbjX-_qMD7CfjmX%2BZD6yq2gKe7%3DM%3Dib5c643vtQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...