Re: [MW:26452] Welders Performance Monitoring

Hi

Repair %= No. of repairs/No. of RT films reviewed *100.

Regards
P Govindan

On Apr 21, 2017 08:48, "ZAIDI Djahid" <djahid.zaidi@gmail.com> wrote:
Dear Gents,

May I get a clarification about the welders performance Monitoring, is it 
by :Defect Inchs/Total inchs Welded
or by :RT Film Rejected/Total RT Film Taken
or by :Defect Inchs/Total Inchs Examinated with RT

For Information the NDT carried out by other subcontractor.

Is there any of that in standards?

Thanks in advance.

D. Zaidi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9dad54ce-1b97-41d1-b203-6312d759df97%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9dWA0-uSh23DXi5rVHFun8i_o-y5FwHn7RiaPLgStaR8Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...