Friday, April 21, 2017

RES: [MW:26454] Welders Performance Monitoring

There are different ways to monitor the welding performance, usually you can use:

 

·         For RT: "Number of rejected films" per "Total Number of films"

·         For UT: "Length of defect" per "Total length inspected"

·         For Joints: "Number of Joints repaired" per "Total number of Joints" or "Number of cut of joints" per "Total number of joints"

 

You shall agree the method and the limits acceptable with your client during the bidding stage of the Project once it can involve high control costs.

 

Best regards

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Em nome de PUB:ZAIDI Djahid
Enviada em: quinta-feira, 20 de abril de 2017 05:16
Para: Materials & Welding
Assunto: [MW:26449] Welders Performance Monitoring

 

Dear Gents,

 

May I get a clarification about the welders performance Monitoring, is it 

by :Defect Inchs/Total inchs Welded

or by :RT Film Rejected/Total RT Film Taken

or by :Defect Inchs/Total Inchs Examinated with RT

 

For Information the NDT carried out by other subcontractor.

 

Is there any of that in standards?

 

Thanks in advance.

 

D. Zaidi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9dad54ce-1b97-41d1-b203-6312d759df97%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...