[MW:26399] Radiography requirement of Annular Plate butt welded joint of the Tank / API 653/650



Dear Experts,

Tank Material - Group 1
Diameter of Tank - 15 meters

Inspection Recommendation - Replacement of Annular Plate wherever thickness loss observed. Mostly 70% Area will be replaced. Currently the Full Bottom Plate replacement is not feasible. 

Configuration of Weld Joint - Single Butt welded joint with backing strip for the Annular Plate joint.

Query 1: Whether Radiography will be required for the butt welded joint as per API 650, Section 8.1.2.9? 
Query 2: If RT will be required and if it is not possible, whether UT can be taken.

Hope to see the response with respect to Code and request specific answer against both the queries.

Thank you
Regards, Vino




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DNAxWAd4Q9N-7OdcnK3auwHC6gPOaNsr2YYXMJ0qtoqg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...