Re: [MW:26433] Radiography requirement of Annular Plate butt welded joint of the Tank / API 653/650

Dear Prasad

Thanks for the response. However, I understand that Section 8.1.2.9 does not refer to RT requirements for Group 1 materials. In that case RT won't be required for butt welded Annular Plate I believe. 


Thanks and Regards 
Vino 
Qatar 




On 16/04/2017 9:29 AM, "Prasad Rode" <purode333@gmail.com> wrote:
Ans1) yes, spot radiography is required with 50% on radial joints.
2) pls check appendix U for the same.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b98fc88-8322-40ea-8ec1-92e8a245b299%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7CpZDQihiwGYs0FjtOym6s%2BvqUr6MOmeog2DmRL5dOYPg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...