I believe you are repairing the tank.

If so, as per clause 12.2.1.4 of API 653, each annular plate joints shall be radiographed where the shell course rests on the annular plate.

Regards
Govindan Perumal

On Apr 17, 2017 04:37, "Vino Varghese" <vinopvarghese@gmail.com> wrote:
Dear Prasad

Thanks for the response. However, I understand that Section 8.1.2.9 does not refer to RT requirements for Group 1 materials. In that case RT won't be required for butt welded Annular Plate I believe. 


Thanks and Regards 
Vino 
Qatar 




On 16/04/2017 9:29 AM, "Prasad Rode" <purode333@gmail.com> wrote:
Ans1) yes, spot radiography is required with 50% on radial joints.
2) pls check appendix U for the same.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b98fc88-8322-40ea-8ec1-92e8a245b299%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7CpZDQihiwGYs0FjtOym6s%2BvqUr6MOmeog2DmRL5dOYPg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9c3vWU2ckUqn2qfFys6Z7nywC%3DvdKEejT12zisVdr%3DVAw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...