In par 10 of ASTM/ASME (S)A403 (Stainless Steel Wrought products) complete procedure and requirements are explained on this issue, no space for discussion
Regards
Jurgen Prinsen IWE/MSc
Weld-Tech vof
Welding Engineering and Consultancy
----- Oorspronkelijk bericht -----
Van: "claire roberston" <jamisburns@hotmail.co.uk>
Aan: "Materials & Welding" <materials-welding@googlegroups.com>
Verzonden: Zondag 23 april 2017 15:44:21
Onderwerp: [MW:26465] Surface Defects on Dish End
A dent in material formation is not a welding defect. Can you include a photo. A weld repair is exactly that! A repair to the welded area. Otherwise it is a fabrication repair. Please clarify
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc4538ad-966e-4e19-9b86-5cafe3318697%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2116178022.12014804.1493024535002.JavaMail.zimbra%40online.nl.
For more options, visit https://groups.google.com/d/optout.
Regards
Jurgen Prinsen IWE/MSc
Weld-Tech vof
Welding Engineering and Consultancy
----- Oorspronkelijk bericht -----
Van: "claire roberston" <jamisburns@hotmail.co.uk>
Aan: "Materials & Welding" <materials-welding@googlegroups.com>
Verzonden: Zondag 23 april 2017 15:44:21
Onderwerp: [MW:26465] Surface Defects on Dish End
A dent in material formation is not a welding defect. Can you include a photo. A weld repair is exactly that! A repair to the welded area. Otherwise it is a fabrication repair. Please clarify
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc4538ad-966e-4e19-9b86-5cafe3318697%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2116178022.12014804.1493024535002.JavaMail.zimbra%40online.nl.
For more options, visit https://groups.google.com/d/optout.
Comments