Sunday, February 28, 2016

RE: [MW:24399] REPAIR OF METAL LOSS BY COLD WELD (BELZONA)

API 570, API 510

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohd Siraj
Sent: Sunday, February 28, 2016 1:56 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:24397] REPAIR OF METAL LOSS BY COLD WELD (BELZONA)

As per API570 &510,
Reapir depend on thickness measurement.

permenant repair shall be done by flushing plate welding/hollow cylinder.

Temporary leak can b arrested by leak clamp.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a835f29-6b91-44ca-b687-c88c59358831%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BAY403-EAS55379CB4ACF43EB22912A0DBB90%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...