Dear Mr Shaunak
Generally Welding Engineer is preparing the above procedure and QCM will approve the same
But as per your mail you are ASME certified company ,so please refer your company's ASME Quality Manual which is approved by ASME Authorised Inspector.
Thanks and Regards
Santosh Gaikwad
Sent from my iPhone
> On 18-Feb-2016, at 2:39 PM, Shaunak Upadhyay <shanupadhyay@gmail.com> wrote:
>
> Dear All,
>
> Please clarify below points, if have reference standard also write in your reply.
>
> 1. PQR in ASME - Certified by Manufacturer
> Who can certified PQR? QC manager or welding engineer?
> In my company no have welding manager. So who can certify PQR.
>
> 2. WPQ in ASME - Certified by Manufacture
> Who can certified?
> Same question as above.
>
> 3. WPS in ASME -
> WPS require approved by QC Manager or welding engineer can approve this ?
>
> Please reply your valuable answer and if have specific ASME clause number let me know.
>
> Thanks in advance.
>
> Regards
> Shaunak.
> shanupadhyay@gmail.com
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d0a84f3d-85a6-4c51-a2ec-a5ea1ae7beb5%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1790AADD-584F-43AB-B3C0-64E3D63747BA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-