Tuesday, February 23, 2016

Re: [MW:24362] dissimilar weld

Materials come with solution annealed/ annealed conditions, consumables do not.
Any way ER NiCr-3 is being advised.
Thanks

Regards,
Manish kulkarni
--------------------------------------------
On Sun, 21/2/16, Ramin Kondori <raminkondori@gmail.com> wrote:

Subject: Re: [MW:24340] dissimilar weld
To: materials-welding@googlegroups.com
Date: Sunday, 21 February, 2016, 9:30 PM

if 625
meets your service requirements, so will ERNiCrMo-3What
I mean is that this filler metal matches the properties of
625 quite well...So if 625 is fit for this
service, ERNiCrMo-3 could be acceptable
too...


Ramin 
KondoriSr. QA/QC & Welding
Engineer-----------------------------------------------------------PG-Dip. in Welding
Engineering (IWE  AT  0070)BSc. in Civil Engineering
(IUT)BGAS Painting
InspectorASNT Level
I&II                   
    

On Sun, Feb 21, 2016 at
4:38 PM, manish kulkarni <kul_manish@yahoo.co.in>
wrote:
But there
are limitations for temp. In spur service for this
consumable.

Sent
from Yahoo Mail on Android

On Sun, 21
Feb, 2016 at 4:13 pm, Ramin Kondori<raminkondori@gmail.com>
wrote: ER NiCrMo-3 will do
the gob



Ramin 
KondoriSr. QA/QC & Welding
Engineer-----------------------------------------------------------PG-Dip. in Welding
Engineering (IWE  AT  0070)BSc. in Civil Engineering
(IUT)BGAS Painting
InspectorASNT Level
I&II                   
    

On Sun, Feb 21, 2016 at
2:18 PM, manish kulkarni <kul_manish@yahoo.co.in> wrote:


 Any suggestions for consumable slection for SS 310S to
cast Inconnel 625 material for sour service and max temp.
exposure 650 Deg.C??

Any corrosion tests for such joints?



Regards,

Manish kulkarni



--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1890907287.6111280.1456051715106.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.






--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUgmUSDpLFWg86XT2N-hFBpmBk4LJNJHdi-NH0cSCT6Xrg%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.




--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1981026294.6150239.1456060085581.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.






--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUi31%3DGhuLoS7jgMDs2NgAzuuZotRq4Svh8JvUUFh6S12Q%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16919437.6929888.1456209657418.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...