Re: [MW:24320] PQR WPQ certified

MANUFACTURER HAS TO CERTIFY AND APPROVE, WITHIN COMPANY , PERSON MAY BE FROM QUALITY, PRODUCTION OR WELDING.

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Thu, Feb 18, 2016 at 5:09 PM, Shaunak Upadhyay <shanupadhyay@gmail.com> wrote:
Dear All,

Please clarify below points, if have reference standard also write in your reply.

1. PQR in ASME - Certified by Manufacturer
Who can certified PQR?  QC manager or welding engineer?
In my company no have welding manager. So who can certify PQR.

2. WPQ in ASME - Certified by Manufacture
Who can certified?
Same question as above.

3. WPS in ASME -
WPS require approved by QC Manager or welding engineer can approve this ?

Please reply your valuable answer and if have specific ASME clause number let me know.

Thanks in advance.

Regards
Shaunak.
shanupadhyay@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d0a84f3d-85a6-4c51-a2ec-a5ea1ae7beb5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmWk-C6k5mve8PX6271o3kiNW0TiXg_FY2mNihQfC3gg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...